wangyi2003 发表于 2006-2-26 11:59:00

镀铬

<P>我来问一个问题:<BR>CR-1与HCR-3在镀铬有什么区别</P>

wangyi2003 发表于 2006-3-17 12:58:00

<P>看来没有人能回答</P>
<P>&nbsp;</P>

旅夜书怀 发表于 2006-3-17 20:02:00

<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">CR-1</FONT>光亮镀铬<BR> <BR>特性与用途:<BR>(<FONT face="Times New Roman">1</FONT>)适用于各种镀铬工艺。<BR>(<FONT face="Times New Roman">2</FONT>)电流效率高,沉积速度。<BR>(<FONT face="Times New Roman">3</FONT>)提高镀液深镀能力和分散能力。<BR>(<FONT face="Times New Roman">4</FONT>)能降低铬酐浓度和操作温度,节省材料和能源。<FONT face="Times New Roman"> </FONT>  <?xml:namespace prefix = o ns = "urn:schemas-microsoft-com:office:office" /><o:p></o:p></P>
<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">&nbsp;<o:p></o:p></FONT></P>
<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">CR-2</FONT>高效率硬铬添加剂<BR><BR>特性与用途:<BR>(<FONT face="Times New Roman">1</FONT>)阴极电流效率高,可达<FONT face="Times New Roman">22-27%</FONT>节约电能。<BR>(<FONT face="Times New Roman">2</FONT>)电流密度范围宽,沉积速度快,省工,省时。<BR>(<FONT face="Times New Roman">3</FONT>)不含氟,无稀土,无阴极低电流密度区腐蚀,无阳极腐蚀。<BR>(<FONT face="Times New Roman">4</FONT>)镀层硬度可达<FONT face="Times New Roman">HV1000</FONT>以上,微裂纹大于<FONT face="Times New Roman">400</FONT>条<FONT face="Times New Roman">/cm</FONT>。<FONT face="Times New Roman">……</FONT>  <o:p></o:p></P>
<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">&nbsp;<o:p></o:p></FONT></P>
<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">CR-3</FONT>黑铬添加剂<BR><BR>特性与用途<FONT face="Times New Roman">:<BR></FONT>(<FONT face="Times New Roman">1</FONT>)可在不锈钢、铜、镍等底层上直接电镀,结合力好。<BR>(<FONT face="Times New Roman">2</FONT>)镀液稳定,配方简单,操作方便。<o:p></o:p></P>
<P class=MsoNormal style="MARGIN: 0cm 0cm 0pt"><FONT face="Times New Roman">&nbsp;<o:p></o:p></FONT></P>CR-53铬雾抑制剂<BR><BR>特性与用途: <BR>(1)能有效抑制铬雾的散发,改善操作环境。<BR>(2)添加量少,使用成本低。<BR>(3)降低铬酐的消耗,节约成本。  

wangyi2003 发表于 2006-3-19 02:03:00

<P>谢谢,你在日资企业吗?</P>
<P>&nbsp;</P>